Powder

Alloys Powder

Grade Name Chemical Composition Powder Type Particle Size Properties and Applications
KLB10103 Ni80Cr20 Ni-20Cr Gas Atomized -45/+15μm APS, HVOF
1. Good bond coat for ceramic top coats
2. Excellent oxidation and corrosion resistant
3. Max. operating temperature 980℃
KLB10104 Inconel 625 Ni-20Cr-9Mo-3.5Nb Gas Atomized -45/+15μm APS, HVOF, Laser cladding, PTA
1. Excellent oxidation and corrosion resistant
2. Used in boilers and in chemical industry
3. Max. operating temperature 1000℃
KLB10105 Inconel 718 Ni-19Cr-18Fe-3Mo-5Nb-0.5Al-1Ti Gas Atomized -45/+15μm APS, HVOF, Laser cladding, PTA
1. Excellent high temperature oxidation and corrosion resistance
2. Used on turbines and chemical equipment
3. Max. operating temperature 700℃
KLB10106 NiC276 Ni-16Cr-16Mo-4W Gas Atomized -45/+15μm HVOF
1. ≤100HRB
2. High temperature corrosion and oxidation resistance; resists crevice corrosion, pitting, sulfuric acid and chlorine
3. Max. operating temperature 980℃
KLB10107 Ni40AA Ni-7.5Cr-1.7B-3.5Si Gas Atomized -45/+15μm PTA, HVOF, Laser cladding
1. HRC 40
2. moderate wear resistance, very good machinability
3. Pistons, valves, pump blades, extrusion screws application
4. Max. operating temperature 650℃
KLB10108 Ni50AA Ni-11Cr-2.2B-3.8Si-3Fe Gas Atomized -45/+15μm PTA, HVOF, Flame spray welding
1. HRC 50
2. High hardness and wear resistance
3. Used in molds, Bearings, pistons
4. Max. operating temperature 650℃
KLB10109 Ni60AA-21 Ni-17.5Cr-3.5B-4.5Si-3Fe Gas Atomized -106/+45μm PTA, HVOF, Laser cladding
1. HRC 60
2. High hardness and wear resistance
3. Pistons, valves, pump blades, extrusion screws application
4. Max. operating temperature 650℃
KLB10110 Ni60AA-4 Gas Atomized -45/+15μm
KLB10111 316L Fe-17Cr-12Ni-2.5Mo Gas Atomized -45/+15μm PTA, HVOF, Laser cladding
1. ≤90HRB
2.Austenitic type stainless steel
3. For protection against corrosion, cavitation, low temperature particle erosion and salvage and repair
4. Max. operating temperature 540 °C
KLB10112 410L Fe-12.5Cr Gas Atomized -45/+15μm PTA, HVOF, Laser cladding
1. ≤183HRB
2. Martensitic type stainless steel
3. For protection against corrosion, cavitation, low temperature particle erosion and salvage and repair
4. Max. operating temperature °C
KLB10113 420 Fe-13Cr Gas Atomized -45/+15μm PTA, HVOF, Laser cladding
1. ≤223HRB
2. Martensitic type stainless steel
3. For protection against corrosion, cavitation, low temperature particle erosion and salvage and repair
4. Max. operating temperature  420 °C
KLB10114 Fe1000 Fe-15Cr-6.5Ni-3B-3Si Gas Atomized -45/+20um HVOF
1. HV  650
2. Oil Industry, For hard surfaces in corrosive wear applications
3. Max. operating temperature 550 °C
KLB10115 Fe55 Fe-18Cr-3Ni-1B-1Si Gas Atomized -150/+53μm Laser cladding
1. HRC 55
2. Enhanced wear and corrosion resistance
3. For hydraulic struts
4. Max. operating temperature 550 °C
KLB10116 Co06 Co-29Cr-4.5W-2Ni-1Si-1C Gas Atomized -45/+15μm PTA, HVOF, Laser cladding
1. HRC 38
2.Engine valves, high temperature pressure valves, turbo engine blades
3.Max. operating temperature 840 °C

Tungsten Carbide Powder

Grade Chemical Composition Powder Type Particle Size Properties and Applications
KLA10015 WC-10Co-4Cr Agglomerated and Sintered -45/+15μm HVOF/HVAF
1. Medium WC                                                                  
2. Max.operating temperature 500 ℃
3. The coating applies to working of valve parts in high pressure and salty environment 
KLA10044 WC-10Co-4Cr Sintered & Crushed -45/+15μm HVOF/HVAF/APS
1. Medium WC                                                                  
2. Max.operating temperature 500 ℃
3. Useable in water based solutions and wet corrosive environments
KLA10046 WC-WB-Co Agglomerated and Sintered -45/+15μm HVOF/HVAF
1. Medium WC
2. Better wear resistance and corrosion resistance in molten metal
3. Apply to Continuous Galvanizing Lines (CGL) 
KLA10054 WC-6Co Agglomerated and Sintered -180+45 μm HVOF/APS 
1. Max. operating temperature 500 ℃
2. Dense, hard coating and good wear, erosion resistance
3. Fine microscopic structure and higher boding strength 
KLA10075 WC-12Co Agglomerated and Sintered -45/+15μm HVOF/APS/HVAF
1. Medium WC
2. Max. operating temperature 500 ℃
3. Coating has the durable wear resistance, erosion resistance and sliding wear resistance
4. Intensive coating and has compact micro structure and high bonding strength
5. Durable oxidation resistance and corrosion resistance                                                                                                                 6. Apply to general wear-out parts, like corrugator roll of paper manufacturing machinery                                                                                                                   
KLA10114 WC-12Co Sintered & Crushed -45/+15μm HVOF/APS
1. Medium WC                                                    
2.  Max.  operating temperature 500 ℃
3. Hard and density coating has excellent wear resistance
4. Apply to machine parts
KLA10122 WC-17Co Agglomerated and Sintered -45/+15μm HVOF, HVAF
1. Medium particle of WC
2. Max.operating temperature 500 ℃
3. Coating has excellent wear resistance, erosion resistance and sliding wear resistance
intensive coating has compact microscopic structure and high bonding strength
4. Excellent toughness of coating
KLA10148 WC-15Ni Agglomerated and Sintered -45/+15μm HVOF
1. Max. operating temperature 500 ℃
 2. Better erosion resistance and toughness than WC-Co coating
KLA10152 WC-17Ni Agglomerated and Sintered -45/+15μm HVOF
1. Max.operating temperature 500 ℃
2. Better erosion resistance and toughness than WC-Co coating
KLA10157 WC-20Cr3C2-7Ni Agglomerated and Sintered -45/+15μm HVOF/HVAF
1. Max. operating temperature 750 ℃
2. Better corrosion resistance and toughness than WC-Co coating
3. Superior oxidation resistance and corrosion resistance than WC-Co coating
4. Apply to gate valve and relevant component
KLA10170 WC-18(NiMoCrFeCo) Agglomerated and Sintered -45/+15μm  HVOF/HVAF
1. Max. operating temperature 500 ℃   
2. The powder with a highly corrosion resistant matrix which is similar to Hastelloy C
3. Better corrosion resistance than WC-Co-Cr and WC-Ni coatings
KLA10177 WC-10Ni-5Cr Agglomerated and Sintered -45/+15μm HVOF
1. Medium particle of WC                                                                  
2. Max. operating temperature 500 ℃
3. The coating applies to working of valve parts in high pressure and salty environment
4. Similar to GP10C
KLA10184 Cr3C2-20NiCr Agglomerated and Sintered -45/+15μm HVOF/HVAF
1. Medium particle of chromium carbide
2. The highest operating temp. is 850℃
3. Compact corrosion resistance and erosion resistance coating
4. Excellent gas corrosion resistance
5. High temperature and gas corrosion resistance.
6. Apply to valve rod, oil drilling core pin, furnace bottom roller in steel industry
KLA10190 Cr3C2-25NiCr Agglomerated and Sintered -45/+15μm HVOF/HVAF
1. Medium particle of chromium carbide
2. Highest operating temp. is 850℃
3. Compact corrosion resistance and erosion resistance coating
4. Excellent gas corrosion resistance
5. High temperature and gas corrosion resistance.
6. Apply to valve rod, oil drilling core pin, furnace bottom roller in steel industry
KLA10201 Cr3C2-37WC-18(NiCrCo) Agglomerated and Sintered -45/+15μm HVOF/HVAF
1. Medium particle of chromium carbide
2. Compact corrosion resistance and erosion resistance coating
3. Higher hardness than GP25NC
4. Hard-Chromium replacement
KLA10207 Cr3C2-7WC-30(NiCr) Agglomerated and Sintered -45/+15μm HVOF/HVAF
1. Medium particle of chromium carbide
2. Compact corrosion resistance and erosion resistance coating
3. Hard-Chromium replacement

Oxide Ceramics

Grade Chemical Composition Powder Type Particle Size Propeties and Applicaions
KLT17082 Al2O3 Fused and Crushed -45/+15µm 1. Purity 99.8+
2. Max. operating temperature 1650°C
3. Excellent dielectric and thermal insulation characteristics, resists wear, chemically inert, stable at high temperatures
4. For corona rolls, capacitors coating
KLT17091 Cr2O3 Sintered and Crushed -45/+15µm 1. Purity 99.5+
2. Max. operating temperature 540°C
3. Hard, corrosion and wear resistant ceramic coatings
4. For anilox rolls in printing machines
KLT17095 TiO2 Sintered and Crushed -45/+15µm 1. Max. operating temperature 540°C
2. Excellent corrosion resistance
3. For wear rings, down-hole plungers, pump components
KLT17098 Y2O3 Agglomerated and Sintered -45/+15µm 1.Excellent dielectric and electrical insulation properties
2.Resistance to thermal shock and high-temperature particle erosion
3.Stable properties under high temperature conditions
4.Wear resistance and chemical inertness
5.Insoluble in acids, bases, and alcohol
6.The maximum operating temperature of the coating is 2000 ℃